To reduceHeat preservation brickporosity, improve the quality of heat preservation brick, rise shape pressure. To brick of common heat preservation, shape pressure should achieve 137MPa; Of brick of high density heat preservation shape pressure should be inside limits of 176 ~ 215MPa. That is to say, the friction that introduces 250t above only presses bricky machine to shape, ability obtains such result. Porosity of heat preservation adobe should achieve following requirements: The ≤ of heat preservation brick such as Ⅰ 21% ; The ≤ of heat preservation brick such as Ⅱ 23% ; The ≤ of heat preservation brick such as Ⅲ 22% before shaping, want to examine model dimension. Model of brick of common heat preservation puts feet rate: Upside 1.5% ; Face of press press of medium, bottom 3.0% ; Be not 1.5% of press press face.